Pre-League MAM14M 14Kt Casting

Pre-League MAM14M 14Kt Casting
Manufacturer: Melt
Call us at +962 6 582 6330 for price

With l`aggiunta 5% Silver Alloy:

Melting Temperature: 870 ° C
P.S .: 12,59 Kg / dm³
HB (Brinell hardness): 140
Corresponding to the color composed as follows: Au 585 Ag 215 Cu 200
Color: Green Yellow

Pre-alloy casting.