Pre-League MACH6 14Kt Casting

Pre-League MACH6 14Kt Casting
Manufacturer: Melt
Call us at +962 6 582 6330 for price

With l`aggiunta 5-10% of Silver in alloy:

Melting Temperature: 918 ° C
P.S .: 12,98 gr / dm³
HB (Brinell hardness): 170
Oxygen content: 10 ppm
Corresponding to the color composed as follows: Au 585 Ag 140 Cu 275
Color: Red

Pre alloy for casting.